Application and Characteristics | Resin Type | Melt Volume Rate, 200 °C/5 kg [cm³/10 min] | Vicat Softening Temperature VST/B/50 (50N, 50 °C/h) [°C] | Flexural Strength, 23 °C [MPa] | Tensile Strain at Break, 23 °C [%] | Light Transmission at 550 nm [%] |
---|---|---|---|---|---|---|
Injection Molding, Very good clarity, Higher melt flow | K-RESIN BK10 | 15 | 53 | 28 | 180 | 91 |
Injection Molding, Very good clarity, High stiffness | K-RESIN KR01 | 8 | 65 | 45 | 15 | 92 |
Injection Molding, Very good clarity, High surface gloss | K-RESIN KR03 | 7.5 | 60 | 30 | 170 | 91 |
Injection Molding, Very good clarity, High surface gloss | K-RESIN KR03E | 7.5 | 60 | 30 | 170 | 91 |
Sheet, Excellent clarity, Blow Molding | K-RESIN KR05 | 7.5 | 60 | 30 | 170 | 91 |
Sheet, Good clarity, Good surface gloss | K-RESIN KR38 | 9 | 50 | 20 | 200 | 90 |
Sheet, Excellent combination of clarity and toughness, High surface gloss | K-RESIN KR40 | 10 | 40 | 17 | 320 | 90 |
Film, High permeation, Good stiffness | K-RESIN KR53 | 10 | 40 | 17 | 320 | 90 |
Resin Grade | Main Applications | Key Characteristics | Chemical Nature and Classification Basis | Wax Content | Special Features |
---|---|---|---|---|---|
KR01 | Injection molding | Lower strength than KR03, but better in bending resistance, toughness, and surface hardness; higher impact resistance than GPPS | - | - | Primarily for injection molding |
KR03 | Injection molding for products without visible gels, sheet extrusion molding | - | Chemically the same as KR05 and KR10; classified by the number of gel/fish eye in the resin | Contains trace wax | Suitable for applications where gel - free final products are required |
KR05 | Blow molding, high - quality sheet extrusion, profile extrusion, injection blow molding | - | Chemically the same as KR03 and KR10; classified by the number of gel/fish eye in the resin | Contains trace wax | Used for various extrusion and blow - molding processes |
KR10 | Film formation | - | Chemically the same as KR03 and KR05; classified by the number of gel/fish eye in the resin (has the least gel content) | Contains wax | Specifically for film - forming applications |
KR03NW | - | - | - | Does not contain wax | - |
KR05NW | - | - | - | Does not contain wax | - |
KK38 | Blending with other resins | Lower optical properties but higher impact strength; can improve economic efficiency by adjusting blending ratio with other resins | - | - | Developed for blending with other resins |
Packaging:
Transportation:
Handling Precautions:
Contact Us: Get in touch to start our collaboration today.
Contact us now to customize packaging and branding exclusively for your company
Q1. Are you a factory or trading company?
Q2. Can I get samples for testing?
A: Yes, we provide samples. Customers cover the initial shipping costs, which are reimbursed in our first cooperation.
Q3. How does your factory ensure quality control?
A: Our factory is ISO9001:2008, REACH, and FAMIQS certified, ensuring rigorous quality control. Each Batch of goods do SGS inspection before leaving our factory.
Q4. What's your Delivery Time?
A: Delivery typically takes 5 to 10 days after payment receipt. Larger orders are confirmed with our production department for prompt, quality-assured delivery.
Q5. What are your payment terms?
A: We accept L/C, T/T, Western Union, and Paypal. Alternative methods can be discussed.
Q6. Which documents do you provide?
A: Standard documents include Commercial Invoice, Price List, Packing List, COA, Origin Certificate, Quality/Quantity Certificate, Beneficiary's Certificate, MSDS, B/L, and others upon request.
Additional Information: